Specifies requirements for three grades of copper wire, which may be plain or tinned and one grade of copper alloy wire for general electrical purposes, supplied in forms other than straight lengths. It does not apply to wires intended for special applications such as those requiring enamelling or textile covering, nor does it apply to wires taken from stranded conductors, either bare or covered or from insulated cables and flexible cords. Chemical composition, mechanical and electrical properties and a hydrogen embrittlement test are specified, and appendices provide information on related specifications and testing.
Published: 05/04/1996
Pages: 12
Table of contents
Cited references
Content history
Table of contents
Header
About this publication
PREFACE
FOREWORD
1 SCOPE AND GENERAL
1.1 SCOPE
1.2 REFERENCED DOCUMENTS
1.3 DEFINITIONS
1.4 DESIGNATION
1.4.1 General
1.4.2 Alloy designation
1.4.3 Temper designation
1.5 ROUNDING OF TEST RESULT VALUES
1.5.1 General
1.5.2 Tensile test results
1.6 PACKAGING
1.7 MARKING
2 SPECIFIC REQUIREMENTS
2.1 SCOPE
2.2 CHEMICAL COMPOSITION
2.3 TEMPER
2.4 MECHANICAL PROPERTIES
2.4.1 General
2.4.2 Tensile requirements for C11000 supplied in the hard temper
2.4.3 Elongation requirements for C11000 supplied in the annealed temper
2.4.4 Tensile requirements for tin-bearing copper (149) in the hard temper
2.5 MANUFACTURING TOLERANCES
2.5.1 Diameter tolerances
2.5.2 Ovality
2.6 ELECTRICAL RESISTIVITY
2.6.1 Plain wire
2.6.2 Tinned wire (applicable to C11000 only)
2.7 HYDROGEN EMBRITTLEMENT RESISTANCE (Applicable to C10100 and C10200 only)
2.8 TINNING (Applicable to C11000 only)
2.9 FREEDOM FROM DEFECTS
2.10 JOINTS
3 TEST METHODS
3.1 SCOPE
3.2 SELECTION AND PREPARATION OF TEST SAMPLES
3.3 CHEMICAL ANALYSIS
3.4 MECHANICAL TESTS
3.5 ELECTRICAL RESISTIVITY TEST
3.6 HYDROGEN EMBRITTLEMENT TEST (applicable to C10100 and C10200 only)
3.7 TINNING TEST (applicable to C11000 only)
3.7.1 General
3.7.2 Preparation of test pieces
3.7.3 Cleaning of helix
3.7.4 Preparation of test solutions
3.7.5 Immersion test
3.7.6 Determination of mass of copper dissolved
3.8 TEST REPORT
APPENDIX A
A1 GENERAL
A2 INFORMATION TO BE SUPPLIED BY THE PURCHASER
APPENDIX B
APPENDIX C
C1 SCOPE
C2 FREQUENCY OF TESTING
C3 ELECTRICAL RESISTIVITY TEST
C3.1 General
C3.2 Specification of values
C4 HYDROGEN EMBRITTLEMENT TEST
Cited references in this standard
[Current]
Metallic materials — Tensile testing — Method of test at room temperature
[Current]
Numerical values — Rounding and interpretation of limiting values
[Superseded]
Methods for the analysis of unalloyed copper, Part 1: Method for the electrolytic determination of copper in unalloyed copper containing not less than 99.85 percent copper
IEC 28
International standard of resistance for copper
[Current]
Copper — Hydrogen embrittlement test
Content history
[Superseded]
DR 95038
AS/NZS 1574:1996 REC:2020
$79.54
AUD
Inclusive of GST
Available formats
iconCreated with Sketch.
Available formats
icon_export/16/closeCreated with Sketch.
Web Reader
Instantly view standards in your browser. Search, bookmark, highlight, and comment for anytime access - online and offline.
Web Reader (PDF)
View standards in PDF format in your browser. Search, bookmark, highlight, and comment for anytime access - online and offline.
Web Reader
Licence:
1 user
Total
$79.54
Add to cart
visa logo
mastercard logo
amex logo