AS 1580.409.2-2002

[Current]

Paints and related materials — Methods of test, Method 409.2: Low temperature coalescence

This Standard sets out a method for determining the ability of a freshly applied latex paint film, typically applied at 30 to 50 µm dry film thickness, to coalesce at temperatures of 5°C to 8°C, after a specified drying period at that temperature.
Published: 13/12/2002
Pages: 3
Table of contents
Cited references
Content history
Table of contents
Header
About this publication
1 Scope
2 Referenced documents
3 Definition
4 Principle
5 Apparatus
5.1 Applicator
5.2 Low temperature chamber
5.3 Magnifying lens
5.4 Test panel
5.5 Thermometer(s)
6 Occupational health and safety guidance
7 Test sample
8 Conditioning of test components
9 Procedure
10 Report
Cited references in this standard
[Current]
Gypsum plasterboard
[Current]
Glossary of paint and painting terms
[Superseded]
Paints and related materials — Methods of test, Method 103.1: Preliminary examination and preparation for testing
[Current]
Paints and related materials — Methods of test, Method 102.1: Sampling procedure
AS 1580.102.2
Paints and related materials—Methods of test, Method 102.2: In-process sampling
Content history
[Superseded]
DR 02265
AS 1580.409.2-2002 Rec:2013

One-time Purchase

Access via web browser on any device
One-time purchase
Single publication
Offline access via PDF^

$45.53 AUD

Inclusive of GST
Format *
iconCreated with Sketch.
Web Reader
Licenses *
iconCreated with Sketch.
1 user
Total$45.53 AUD
Add to Cart
IMPORTANT